MIMにおけるAlSl4600鋼の黒鉛添加による炭素量制御 Carbon Control of MIM AlSl 4600 Steels by Graphite Addition

この論文にアクセスする

この論文をさがす

著者

抄録

Debinding process as well as carbon in alloy powder has great effects on carbon content in final products using MIM process.<BR>This paper describes the behavior of carbon and oxygen in debinding and sintering process by varing amount of graphite addition in AISI 4600 steel compounds.<BR>The results are summarized as follows:<BR>(1) Proper amount of carbon and oxygen in compounds makes possible to progress their removal by CO reaction in sintering process.<BR>(2) Graphite addition to AISI 4600 steel compounds enables the control of carbon and oxygen content in fmal products under proper debinding conditions.

収録刊行物

  • 粉体および粉末冶金  

    粉体および粉末冶金 44(5), 411-415, 1997-05-15 

    Japan Society of Powder and Powder Metallurgy

参考文献:  6件

参考文献を見るにはログインが必要です。ユーザIDをお持ちでない方は新規登録してください。

各種コード

  • NII論文ID(NAID)
    10002013776
  • NII書誌ID(NCID)
    AN00222724
  • 本文言語コード
    JPN
  • 資料種別
    ART
  • ISSN
    05328799
  • NDL 記事登録ID
    4205758
  • NDL 雑誌分類
    ZP41(科学技術--金属工学・鉱山工学)
  • NDL 請求記号
    Z17-274
  • データ提供元
    CJP書誌  NDL  J-STAGE 
ページトップへ