The development of new anti-wear steels instead of gray cast iron has been carried out as one measure strengthening the piston-ring. Using the anti-wear steel, wear test and scuffing test were carried out. The test results of the anti-wear steel were compered wtih that of gray cast iron.<BR>The main results are in the following: Wear amount of the anti-wear steel was lower than that of gray cast iron. The anti-wear steel had relatively large variations of scuffing test results. It was necessary for the anti-wear steel with surface modification, as the initial surface break in condition of the steel was not always sufficient. If the initial surface break in condition of the anti-wear steel is improved by surface modifications, the good surface running condition will be achieved without scuffing damage.

収録刊行物

  • 日本舶用機関学会誌  

    日本舶用機関学会誌 31(7), 389-399, 1996-07-01 

    The Japan Institute of Marine Engineering

参考文献:  4件

参考文献を見るにはログインが必要です。ユーザIDをお持ちでない方は新規登録してください。

被引用文献:  2件

被引用文献を見るにはログインが必要です。ユーザIDをお持ちでない方は新規登録してください。

各種コード

  • NII論文ID(NAID)
    10002040948
  • NII書誌ID(NCID)
    AN00196373
  • 本文言語コード
    JPN
  • 資料種別
    ART
  • ISSN
    03883051
  • NDL 記事登録ID
    3994620
  • NDL 雑誌分類
    ZN24(科学技術--運輸工学--船舶)
  • NDL 請求記号
    Z16-747
  • データ提供元
    CJP書誌  CJP引用  NDL  J-STAGE 
ページトップへ