Development of Piston-Ring for Marine Diesel Engine
-
- Miura Kenzo
- 三井造船 (株) 玉野研究所
-
- Okamoto Hitoshi
- 三井造船 (株) 玉野研究所
-
- Jibiki Tatsuhiro
- 三井造船 (株) 玉野研究所
-
- Tanaka Takao
- 三井造船 (株) ディーゼル事業部
-
- Tanaka Masaki
- 三井造船 (株) ディーゼル事業部
Bibliographic Information
- Other Title
-
- 舶用ディーゼル機関ピストンリングの開発
- ハクヨウ ディーゼル キカン ピストン リング ノ カイハツ
Search this article
Abstract
The development of new anti-wear steels instead of gray cast iron has been carried out as one measure strengthening the piston-ring. Using the anti-wear steel, wear test and scuffing test were carried out. The test results of the anti-wear steel were compered wtih that of gray cast iron.<BR>The main results are in the following: Wear amount of the anti-wear steel was lower than that of gray cast iron. The anti-wear steel had relatively large variations of scuffing test results. It was necessary for the anti-wear steel with surface modification, as the initial surface break in condition of the steel was not always sufficient. If the initial surface break in condition of the anti-wear steel is improved by surface modifications, the good surface running condition will be achieved without scuffing damage.
Journal
-
- JOURNAL OF THE MARINE ENGINEERING SOCIETY IN JAPAN
-
JOURNAL OF THE MARINE ENGINEERING SOCIETY IN JAPAN 31 (7), 389-399, 1996
The Japan Institute of Marine Engineering
- Tweet
Details 詳細情報について
-
- CRID
- 1390282680138039552
-
- NII Article ID
- 10002040948
-
- NII Book ID
- AN00196373
-
- ISSN
- 18844758
- 03883051
-
- NDL BIB ID
- 3994620
-
- Text Lang
- ja
-
- Data Source
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed