Synthesis of high-TiO2 pyrope-grossular garnet at 10 GPa.
-
- SATO Kiminori
- Institute for Study of the Earth's Interior, Okayama University
-
- ONUMA Kosuke
- Institute of Mineralogy, Petrology and Economic Geology, Tohoku University
-
- OHTANI Eiji
- Institute of Mineralogy, Petrology and Economic Geology, Tohoku University
-
- KATO Takumi
- Institute of Geoscience, University of Tsukuba
Bibliographic Information
- Other Title
-
- 10 GPaにおける高TiO<sub>2</sub>ざくろ石の合成
- Synthesis of high-TiO2 pyrope-grossular
Search this article
Abstract
A high-titanium containing garnet, SiO2(40.6), TiO2(6.3), Al2O3(18.8), MgO(14.3), CaO(20.21), (wt%) has been synthesized at 10 GPa and 1500°C. Unit cell parameter of this synthetic garnet is determined to be 11.812 Å by micro-focused X-ray diffractmetry and this value is intermediate between those of pyrope and grossular. These results indicate that pyrope-grossular garnet potentially can accommodate TiO2 up to 6.3 wt% at the high of 10 GPa.
Journal
-
- JOURNAL OF MINERALOGY, PETROLOGY AND ECONOMIC GEOLOGY
-
JOURNAL OF MINERALOGY, PETROLOGY AND ECONOMIC GEOLOGY 91 (12), 455-458, 1996
Japan Association of Mineralogical Sciences
- Tweet
Details 詳細情報について
-
- CRID
- 1390001206233952768
-
- NII Article ID
- 10002088443
-
- NII Book ID
- AN10047992
-
- COI
- 1:CAS:528:DyaK2sXhtFylsrs%3D
-
- ISSN
- 18813275
- 09149783
-
- NDL BIB ID
- 4127397
-
- Text Lang
- en
-
- Data Source
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed