Precisions of Wire-EDM are spoiled by a wire deflection and a wire vibration during the machining. Examples, these wire behaviors cause a smoothed corner or a smaller radius corner shape and a concave cut wall.<br>As well known, these wire behaviors are caused by a explosive pressure, a electrostatic force, a electromagnetic force by each discharge and a force caused by flushing of water during Wire-EDM.<br>In previous some papers, wire behaviors are measured and discussed. And other papers reported methods to solve problems of cutting precisions.<br>But in spite of these reports, wire behaviors and the influence of EDM conditions on them are not so cleared, also the relation between cutting accuracy and wire behaviors is not so well understood yet.<br>For these investigations, simulations of Wire-EDM will be useful. But the simulation of Wire-EDM is quite different from them of conventional EDM because all process and repetition from voltage supply to discharge, explosion, machining and wire movement should be considered.<br>In this report we mainly describe a simulating procedure and few nalyzed results of Wire-EDM.

Journal

Citations (9)*help

See more

References(12)*help

See more

Details 詳細情報について

  • CRID
    1390001206233585024
  • NII Article ID
    10002439496
  • NII Book ID
    AN00151681
  • DOI
    10.2526/jseme.29.62_40
  • ISSN
    18810888
    0387754X
  • Text Lang
    ja
  • Data Source
    • JaLC
    • Crossref
    • CiNii Articles
  • Abstract License Flag
    Disallowed

Report a problem

Back to top