Abstract
To utilize pisolite ores as raw materials of iron ore sinter, a commercial production trial was carried out by designing the structure of quasi-particles. Main results obtained from the trial are summarized as follows:<br>(1) The commercial production test using 40 mass% pisolite ores in raw materials showed that high quality sinter was produced by making quasi-particles having duplex structures; the inner core is granulated by raw materials containing the pisolite ores and the outer shell is coated with both coke fine and high grade magnetite ore fines. <br>(2) According to the reduction kinetic analysis of sinter products, high reducibility of the products produced from quasi-particles having the duplex structure results in the improved reduction rate parameters resulting from the product structures containing many micro-pores ranged from 10 to 100μm.<br> (3) Improved reduction degradation characteristics of the products depend on decreased hematite phase and increased magnetite phase in the sinter structures as well as micro-pore distributions.
Journal
-
- ISIJ International
-
ISIJ International 37 (11), 1066-1071, 1997
The Iron and Steel Institute of Japan
- Tweet
Keywords
Details 詳細情報について
-
- CRID
- 1390282681428263168
-
- NII Article ID
- 10002457446
-
- NII Book ID
- AA10680712
-
- COI
- 1:CAS:528:DyaK1cXht1Sisg%3D%3D
-
- ISSN
- 13475460
- 09151559
- http://id.crossref.org/issn/09151559
-
- Text Lang
- en
-
- Data Source
-
- JaLC
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed