Boronizing in the fluidized bed was performed on the surface treatment of austenitic spheroidal graphite cast iron. Tests were carried out on the hardness, microscopy. X-ray diffractometry, electron microprobe X-ray analysis, glow discharge spectrometry, friction and wear characteristic, and the corrosion behaviors in boronized specimens. As a result, the boride layer in the austenitic spheroidal graphite cast iron produced by fluidized bed was 1400 HK in hardness and consisted of two intermetaltic compounds (FeB, Fe2B), The enrichment of Si and Ni excluded from the horonized compound was detected like the stripe. The boride layer more improved friction properties and the wear resistance of austenitic spheroidal graphite cast iron than those of SUS304 and Al2O3. The corrosion resistance against 0.1 N HCl and 0.1 N H2SO4 of the boronized specimen was more improved compared to untreated specimens. It was found that the boronizing method in fluidized bed could be successfully applied to the surface treatment of austenitic spheroidal graphite cast iron.
Journal
-
- Journal of Japan Foundry Engineering Society
-
Journal of Japan Foundry Engineering Society 70 (5), 303-308, 1998
Japan Foundry Engineering Society
- Tweet
Keywords
Details 詳細情報について
-
- CRID
- 1390282681485230848
-
- NII Article ID
- 10002553754
-
- NII Book ID
- AN10514770
-
- ISSN
- 21855374
- 13420429
-
- NDL BIB ID
- 4470660
-
- Text Lang
- en
-
- Data Source
-
- JaLC
- NDL
- CiNii Articles
-
- Abstract License Flag
- Disallowed