AC4B アルミニウム合金円筒状鋳物T6材の機械的性質および組織に及ぼす質量効果の影響 Mass effect on the mechanical properties and strucure of AC4B aluminum alloy cylindrical castings subjected to solution treatment

この論文にアクセスする

この論文をさがす

著者

抄録

The tensile strength and structure (dendrite arm spacing or D.A.S) of cylindrical castings were determined for specimens with different thicknesses and masses subjected to the T6 solution treatment, because they are expected to be affected by the casting modulus (volume/surface area) and the cooling rate (solidification time). When <i>V/S</i> of the castings increases, the cooling rate and the strength decreased, but D.A.S increases. The strength and D.A.S can be presented as a function of the nth power of the casting modulus <i>(V/S)</i>.

収録刊行物

  • 軽金属  

    軽金属 48(12), 608-612, 1998-12-30 

    The Japan Institute of Light Metals

参考文献:  29件

参考文献を見るにはログインが必要です。ユーザIDをお持ちでない方は新規登録してください。

各種コード

  • NII論文ID(NAID)
    10002665578
  • NII書誌ID(NCID)
    AN00069773
  • 本文言語コード
    JPN
  • 資料種別
    ART
  • ISSN
    04515994
  • NDL 記事登録ID
    4629139
  • NDL 雑誌分類
    ZP41(科学技術--金属工学・鉱山工学)
  • NDL 請求記号
    Z17-284
  • データ提供元
    CJP書誌  NDL  J-STAGE 
ページトップへ