- Sakata Kimiaki
- Specialty Steel Engineering Department, Production Engineering Division 1, Aichi Steel Co. Ltd.
この論文をさがす
抄録
We established the refining technology for cleanliness in regard to austenite type stainless steel. But immersion nozzle clogging in continuous casting occurred by formation of spinel (MgO–Al2O3) type inclusions in strong reduction refining for cleanliness. Therefore, we estimated the conditions for formation of spinel and it was possible to improve the castability while keeping cleanliness by controlling of inclusion compositions.
収録刊行物
-
- ISIJ International
-
ISIJ International 46 (12), 1795-1799, 2006
一般社団法人 日本鉄鋼協会