水素極保湿方法の違いによるPEFCの出力持続性の検討

書誌事項

タイトル別名
  • On contiguity of output power for operating time in hydrogen pole which is moistened by different methods

この論文をさがす

抄録

We know that polymer electrolyte fuel cell (PEFC) can't run for a long time without humidification. As nafion membrane's function deteriorates when hydrogen ions go through in the dried electrodes,we operated PEFC by two methods for a long time. One is a method to apply the water-soluble macromolecule that is Methyl cellulose (MC) to the surface of PEFC. Another is supply the humidified hydrogen in PEFC. We investigate that a cause of the decreasing output is the platinum catalyst of the electrode particles. It is observed that the particle size of the platinum have increased after operation compared with before operation. Also, the platinum catalyst size distribution supported on acetylene change from uniform to non-uniform. In addition to them, we confirm the resolution of MC which apply to the surface of PEFC by STEM.<br>As the result, it was the confirmation that output decrease by particle size and distribution of the platinum catalysts.

収録刊行物

参考文献 (1)*注記

もっと見る

キーワード

詳細情報 詳細情報について

  • CRID
    1390001204341030272
  • NII論文ID
    10021874962
  • NII書誌ID
    AA11948435
  • DOI
    10.2978/jsas.19.59
  • ISSN
    18813917
    09155651
  • データソース種別
    • JaLC
    • Crossref
    • CiNii Articles
  • 抄録ライセンスフラグ
    使用不可

問題の指摘

ページトップへ