145 成型コークスの熱間性状の改善 (2) : 二段加熱による新成型コークス製造法の開発 VII(コークス製造・コークス炉内性状, 製銑, 日本鉄鋼協会 第 102 回(秋季)講演大会)  [in Japanese] 145 Improvement of the strength after CO_2 gasification of formed coke (2) : New development of formed coke process by two-stage heating VII(IRONMAKING)  [in Japanese]

Journal

Tetsu- to- Hagane   [List of Volumes]

Tetsu- to- Hagane 67(12), S795, 1981-09-10  [Table of Contents]

The Iron and Steel Institute of Japan (ISIJ)

Cited by:  1

You must have a user ID to see the cited references.If you already have a user ID, please click "Login" to access the info.New users can click "Sign Up" to register for an user ID.