Si_3N_4-Si_2N_2Oコンポジットの機械的性質に及ぼす粒界相の影響  [in Japanese] Effect of Intergranular Phase on Mechanical Properties of Si_3N_4-Si_2N_2O Composites  [in Japanese]

Abstract

Ce/Si ratio increased with the formation of Si_2N_2O in Ce-doped Si_3N_4 based ceramics with SiO_2 addition. The intergranular liquid remained as a glass on cooling until the ratio exceeded a certain level when the intergranular liquid crystallized as cerium nitrogen apatite (Ce_5(SiO_4)_3N-Ce_<4.67>(SiO_4)_3O) during cooling. There were large differences in flexural strength, fracture toughness between the specimens with the intergranular glassy phase and the ones with the intergranular crystalline phase. Mechanical properties of the bulk bodies depended on those of the intergranular phases.

Journal

Journal of the Ceramic Society of Japan   [List of Volumes]

Journal of the Ceramic Society of Japan 100(1165), 1169-1171, 1992-09-01  [Table of Contents]

The Ceramic Society of Japan

Preview

Preview

Codes

  • NII Article ID (NAID) :
    110002290095
  • NII NACSIS-CAT ID (NCID) :
    AN10040326
  • Text Lang :
    JPN
  • ISSN :
    09145400
  • NDL Article ID :
    3784256
  • NDL Source Classification :
    無機化学・無機化学工業--セラミックス
  • NDL Source Classification :
    ZP9(科学技術--化学・化学工業--無機化学・無機化学工業--セラミックス・窯業)
  • NDL Call No. :
    Z17-249
  • Databases :
    NDL  NII-ELS  Journal@rchive