A new ultra-fine piercing which had been proposed, have been conducted successfully, but has a few troublesome points. A die material is mild steel, and than a coupling of a die and a pierced material is that of metals. Therefore, pierced scrap accumulated in a die hole and stops a punch advancement. If the pierced material rises up unevenly from the die, a horizontal force acts on the punch and the punch defects, advances deviately and shaves the surface of the die hole. These were conquered by means of setting a vacuum chamber under the die. A scrap is sucked away from a die hole at each stroke and a foil of pierced material is pulled down through two holes remoted by 1 mm from the die hole. Thus a high precision and continuous process of the ultra-fine piercing is carried out.
収録刊行物
-
- 日本機械学会論文集C編
-
日本機械学会論文集C編 68 (667), 987-992, 2002
一般社団法人 日本機械学会
- Tweet
キーワード
詳細情報 詳細情報について
-
- CRID
- 1390001206357416576
-
- NII論文ID
- 130004084489
- 110002378434
-
- NII書誌ID
- AN00187463
-
- ISSN
- 18848354
- 03875024
-
- HANDLE
- 2237/9031
-
- NDL書誌ID
- 6118094
-
- 本文言語コード
- ja
-
- データソース種別
-
- JaLC
- IRDB
- NDL
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可