315 ショットピーニング処理によるAC4CH材の高サイクル疲労特性改善(OS1-3 表面改質処理と疲労強度)(OS1 高強度材・表面改質材の疲労と破壊)  [in Japanese] 315 The Improvement of High Cycle Fatigue Properties of AC4CH Alloy with Shot Peening  [in Japanese]