74.改質褐炭のCWM化

DOI

書誌事項

タイトル別名
  • 74. Preparation of CWM from Upgraded Low-Rank Coals

抄録

Several Australian low rank coal were upgraded by hydrothermal treatment process at 200℃-300℃. As the heat-treatment temperature (HTT) was raised, the slurriability of CWM which was prepared from treated coal was improved dramatically. By the DSC measurement, the amount of bound water in CWM decreased with increasing of HTT. From these results, we found that the amount of the bound water was in good agreement with the slurriability of CWM.

収録刊行物

詳細情報 詳細情報について

  • CRID
    1390001205769398400
  • NII論文ID
    110006857319
  • DOI
    10.20550/jiesekitanronbun.36.0_313
  • ISSN
    24238309
    24238295
  • 本文言語コード
    ja
  • データソース種別
    • JaLC
    • CiNii Articles
  • 抄録ライセンスフラグ
    使用不可