  • Creep of dental zirconium oxide at high temperature

この論文をさがす

抄録

The creep of a dental pre-sintered yttrium-stabilized zirconium oxide during sintering was determined by the manner of sag-resistance measurement. inColis ZI (Sirona Dental Systems GmbH) was used. The each specimen is having 0.55mm, 1.15mm and 1.55mm thickness, 5.5mm width and 39mm long. They deformed by the load of 0g, 0.5g and 1.0g respectively on the 20mm span during sintering at 1,450℃. The deformation was remarkable in the thin specimen, which occurred even in the no load.