抄録
In order to determine the effect of addition of selenium and tellurium on the activity coefficient of oxygen, γo, in liquid copper at 1373 K, the modified coulometric titrations described previously have been performed by using an electrochemical cell: O in liquid Cu–Se or Cu–Te solutions/ZrO2(+CaO)/Air, Pt.<BR>The γo value for liquid copper is linearly lowered by the addition of those elements up to NSe=0.02 and NTe=0.03, although the Se–O and Te–O bonds are likely to be weaker than the Cu–O bond. The interaction parameters of selenium and tellurium to oxygen are evaluated from the data to be −13.8 and −16.2 at 1373 K.
収録刊行物
-
- Transactions of the Japan Institute of Metals
-
Transactions of the Japan Institute of Metals 24 (3), 132-138, 1983
社団法人 日本金属学会
- Tweet
キーワード
詳細情報 詳細情報について
-
- CRID
- 1390282680095076992
-
- NII論文ID
- 130003486047
-
- COI
- 1:CAS:528:DyaL3sXitF2murw%3D
-
- ISSN
- 24324701
- 00214434
-
- 本文言語コード
- en
-
- データソース種別
-
- JaLC
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可