熱影響部の脆化について(第9報)

DOI

書誌事項

タイトル別名
  • On the Brittleness of Heat-Affected Zone (Report 9)
  • Brittle Range Related to the Directionality of the Steel Plate
  • 鋼材の圧延異方性と脆化領域

抄録

Distribution of the toughness in the neighbour of weld, depending on the hysteresis and the directionality of the steel plate, are examined. Usability of the "Synthetic Impact Test Specimens" are considered. Max. brittle ratio of the heat-affected zone of the full-annealed steel plate seems to be greater than that of as-rolled steel plate. Synthetic impact values are greater slightly than the calculated one derived from the common impact method.

収録刊行物

  • 溶接学会誌

    溶接学会誌 25 (8), 438-444, 1956

    一般社団法人 溶接学会