抄録
Recent studies of fretting wear are reviewed on the basis of work carried out by the author's laboratory. Some of the new findings are introduced below. (1) The critical amplitude to produce severe wear is equivalent to the amplitude when the non-slip region disappears in the elastic contact. (2) An induction period, the number of fretting cycles to produce damage, is identified. (3) Fretting wear of steel takes place at the point of the maximum strain-energy on the surface and the fatigue crack of glass occurs at the point of the repeated maximum principal stress on the surface arising from the fretting motion. Some methods to prevent fretting damage are also introduced regarding their theoretical and experimental aspects.
収録刊行物
-
- JSME international journal. Ser. 3, Vibration, control engineering, engineering for industry
-
JSME international journal. Ser. 3, Vibration, control engineering, engineering for industry 31 (3), 487-493, 1988
一般社団法人 日本機械学会
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1390282679654479616
-
- NII論文ID
- 130003964257
-
- ISSN
- 09148825
-
- 本文言語コード
- en
-
- データソース種別
-
- JaLC
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可