液体急冷法で作製したSm(Co,Fe,Ni,Cu)7薄帯の磁気特性と構造

書誌事項

タイトル別名
  • Magnetic Properties and Structures of Sm(Co, Fe, Ni, Cu)<sub>7</sub> Ribbons Rapidly Quenched from the Melt

抄録

The structure and magnetic properties of Sm(Co, Fe, Ni, Cu)7 ribbons prepared by a rapid quenching tecnique are investigated with successive annealing at various temperatures. A maximum coercivity of about 6 kOe is obtained for the specimen aged by two steps, namely aged at 800°C for 4 hours and then annealed at 600°C for 3 hours. The cellular precipitate structure composed of 2-17 and 1-5 phases is found in samples with high coercivity. This aging behaviour is very close to that of the sintered alloy with the same composition.