Mechanical milling effects on the crystal structures and magnetic features in some Mn based alloy and compounds Mn基合金および化合物の構造や磁性におよぼすメカニカルミリングの効果
この論文にアクセスする
この論文をさがす
著者
書誌事項
- タイトル
-
Mechanical milling effects on the crystal structures and magnetic features in some Mn based alloy and compounds
- タイトル別名
-
Mn基合金および化合物の構造や磁性におよぼすメカニカルミリングの効果
- 著者名
-
殷, 福星
- 著者別名
-
イン, フクセイ
- 学位授与大学
-
甲南大学
- 取得学位
-
博士 (理学)
- 学位授与番号
-
乙第10号
- 学位授与年月日
-
1997-03-14
注記・抄録
博士論文
目次
- Contents / C-1 / (0003.jp2)
- Preface / Pr-1 / (0005.jp2)
- Acknowledgment / Ac-1 / (0007.jp2)
- Chapter1.Introduction. / p1 (0008.jp2)
- §1.1.Recent development in mechanical alloying and mechanical milling / p1 (0008.jp2)
- §1.2.Crystal structures and magnetic features of the magneto-ordered alloys and compounds containing Mn / p6 (0011.jp2)
- §1.3.Destinations for the present research / p10 (0013.jp2)
- §1.4.Experimental procedures / p13 (0014.jp2)
- §1.5.References for chapter1 / p15 (0015.jp2)
- Chapter2. Disordering characteristics of the τ-phases in Mn-Al-X(X=C and Ga) alloys during mechanical milling. / p18 (0017.jp2)
- §2.1.Introduction / p18 (0017.jp2)
- §2.2.Microstructures of the τ-phases evolved during mechanical milling / p19 (0017.jp2)
- §2.3.Magnetizations and the ordering degrees in the milled τ-phases / p22 (0019.jp2)
- §2.4.Discussion on atomic diffusion routs during mechanical milling / p24 (0020.jp2)
- §2.5.Summaries / p27 (0021.jp2)
- §2.6.References for chapter2 / p27 (0021.jp2)
- Chapter3. The different disordering features of B2 type κ-phase and L2₁ type Heusler phase in Cu-Mn-Al alloy system during mechanical milling. / p28 (0022.jp2)
- §3.1.Introduction / p28 (0022.jp2)
- §3.2.Microstructure and magnetic characteristics of the κ-phase and Heusler alloys during mechanical milling / p31 (0023.jp2)
- §3.3.The disordering mode and lattice constant of the κ-phase during milling / p33 (0024.jp2)
- §3.4.Thermal recoveries of crystal structure and magnetic features in the milled alloys / p36 (0026.jp2)
- §3.5.Summaries / p38 (0027.jp2)
- §3.6.References for chapter3 / p39 (0027.jp2)
- Chapter4.Mechanical milling consequences in crystal structure and magnetic features of some Cu₂Sb type intermetallic compounds. / p40 (0028.jp2)
- §4.1.Introduction / p40 (0028.jp2)
- §4.2.Crystallographic characters of the C38 (Cu₂Sb)type structure and the changes of lattice constants during mechanical milling / p42 (0029.jp2)
- §4.3.Microstructure features altered during milling in the compounds / p45 (0030.jp2)
- §4.4.Magnetic properties of milled compounds and discussion on the structural modification concerning the magnetic variations / p48 (0032.jp2)
- §4.5.Summaries / p52 (0034.jp2)
- §4.6.References for chapter4 / p53 (0034.jp2)
- Chapter5. Effects of composition on the mechanical milling products in the B8₁ type non-stoichiometric MnSb intermetallic compounds. / p54 (0035.jp2)
- §5.1.Introduction / p54 (0035.jp2)
- §5.2.Microstructure features in ball milled MnSb and Mn₀.₅₅Sb₀.₄₅ compounds. / p57 (0036.jp2)
- §5.3.Magnetic behaviors for milled MnSb and Mn₀.₅₅Sb₀.₄₅ compounds / p59 (0037.jp2)
- §5.4.Lattice deformation and anti-site disordering in MnSb compound occurred during milling / p61 (0038.jp2)
- §5.5.Behaviors of Mn₀.₅₂Sb₀.₄₈ compound in a more intensive milling condition. / p63 (0039.jp2)
- §5.6.Summaries / p65 (0040.jp2)
- §5.7.References for chapter5 / p66 (0041.jp2)
- Chapter6.Milling induced anti-site disordering and its effects on the first-order phase transition in the B8₁(NiAs)type MnAs and MnBi intermetallic compounds. / p68 (0042.jp2)
- §6.1.Introduction / p68 (0042.jp2)
- §6.2.Microstructure features of MnAs and MnBi compounds duringmechanical milling / p70 (0043.jp2)
- §6.3.Magnetic features and unit cell dimensions in milled MnAs and MnBi compounds / p74 (0045.jp2)
- §6.4.A phenomenological approach to the milling effects on atomic configurations in MnAs compound / p77 (0046.jp2)
- §6.5.Structure factor analysis on the atomic transition mode during milling of MnBi compound / p81 (0048.jp2)
- §6.7.References for chapter6 / p85 (0050.jp2)
- Chapter7.Phase transitions of orthorhombic type structured nano-crystalline MnP and MnB compounds during mechanical milling. / p87 (0051.jp2)
- §7.1.Introduction / p87 (0051.jp2)
- §7.2.Microstructural characteristics of the milled MnP and MnB compounds / p89 (0052.jp2)
- §7.3.Lattice distortion and magnetic features in milled MnP and MuB compounds / p93 (0054.jp2)
- §7.4.Characteristics of milling induced phase transformations in MnP and MnB compounds / p99 (0057.jp2)
- §7.5.Summaries / p101 (0058.jp2)
- §7.6.References for chapter7 / p102 (0059.jp2)
- Chapter8.Amorphous phases of perovskite type Mn₃MC(M=Al,Zn and Ga)carbides formed during mechanical milling and their annealing effects. / p103 (0059.jp2)
- §8.1.Introduction / p103 (0059.jp2)
- §8.2.Microstructure and crystal structures of the carbides during milling / p105 (0060.jp2)
- §8.3.Magnetic properties of Mn₃MC compounds during mechanical milling / p108 (0062.jp2)
- §8.4.DSC characterization of the milling induced amorphous phases in the perovskite carbides / p110 (0063.jp2)
- §8.5.Thermal features of further milled amorphous Mn₃AlC and the crystalline products after annealing / p112 (0064.jp2)
- §8.6.Summaries / p116 (0066.jp2)
- §8.7.References for chapter 8 / p116 (0066.jp2)
- Chapter9.Discussions on some common behaviors of the Mn involved alloys and compounds during mechanical milling and concluding remarks. / p118 (0067.jp2)
- §9.1.Regulations of crystalline grain refining and lattice strain accumulating of the Mn alloys and compounds during mechanical milling / p118 (0067.jp2)
- §9.2.Magnetic properties of the magneto-ordered alloys and compounds changed during mechanical milling / p121 (0068.jp2)
- §9.3.Mechanical milling induced lattice distortion and disordering in the Mn involved alloys and compounds / p127 (0071.jp2)
- §9.4.Phase transformations in the alloys and compounds occurred during mechanical milling / p130 (0073.jp2)
- §9.5.References for chapter 9 / p135 (0075.jp2)
- List of figures / p137 (0076.jp2)
- Structural and Magnetic Properties of Mechanically Deformed Heusler Alloys / p669 (0081.jp2)
- Sintering Formation of Low Temperature Phase MnBi and Its Disordering in Mechanical Milling / p335 (0086.jp2)
- Mechanical Milling Effect on Crystal Structures and Magnetic Properties of MnAs and Mn₀.₈Ti₀.₂As Compounds / p1356 (0094.jp2)
- FORMATION OF Bf TYPE NANOCRYSTALLINE MnB IN MECHANICAL MILLING AND ITS MAGNETIC FEATURES / p629 (0098.jp2)
- Structural Evolution of the Mn₀.₅₂Sb₀.₄₈ Compound during High Energy Ball Milling / p1 (0103.jp2)
- Characteristics of Amorphous Mn₃AlC Phases Formed by Mechanical Milling / p1 (0108.jp2)
- CRYSTAL STRUCTURAL TRANSITIONS OF FeSb ANTIMONIDE POWDER IN BALL MILLING / p148 (0112.jp2)
- Effects of Self-Accommodation and Plastic Accommodation in Martensitic Transformations and Morphology of Martensites / (0115.jp2)
- Characterization of the Formation of α₁ Plates from the β₃ Phase in a Cu-Zn-Au Alloy / (0122.jp2)