Apatite Coating on Organic Polymers by a Biomimetic Process

抄録

<jats:p>Dense and uniform layers of a biologically active carbonate‐containing hydroxyapatite can be formed on various kinds of organic polymers by the following biomimetic method. First, a substrate is set in contact with particles of CaO–SiO<jats:sub>2</jats:sub>‐based glass soaked in a simulated body fluid (SBF) with ion concentrations nearly equal to those of human blood plasma for forming the apatite nuclei on the substrate. Second, the substrate is soaked in another solution highly supersaturated with respect to the apatite, e.g, with ion concentrations 1.5 times those of SBF (1.5SBF) for making the apatite nuclei grow on the substrate <jats:italic>in situ.</jats:italic> The induction period for the apatite nucleation, which is defined as the time of the first treatment required for forming enough of the apatite nuclei to make the continuous layer after the second treatment, was almost 24 h for most of the examined polymers. The adhesive strength of the formed apatite layer to the polymers was as high as 3 to 4 M Pa for poly(ethylene terephthalate), poly‐ether sulfone, and poly (vinyl alcohol) hydrogel. This type of apatite–organic polymer composite is expected to be useful for repairing not only living hard tissues but also soft ones.</jats:p>

収録刊行物

被引用文献 (50)*注記

もっと見る

詳細情報 詳細情報について

問題の指摘

ページトップへ