Search Results1-2 of  2

  • 油原 晋 ID: 9000000155968

    川崎製鉄(株)製鉄プラント事業部 (1999 from CiNii)

    Articles in CiNii:1

    • Improvement of Slab Quality by Static Magnetic Field (Development of FC Mold II) (1999)
  • Yuhara Susumu ID: 9000002994479

    Mizushima Works, Kawasaki Steel Corp. (2000 from CiNii)

    Articles in CiNii:3

    • Technology for prevention of internal cracking in slab at Mizushima No.4 Continuous Caster (1999)
    • H2 & N2 mixed gas heating technology to reduce oxygen contamination of recycled Tundish (Development of reducing oxygen contamination of recycled Tundish-1) (2000)
    • 154 Analysis of secondary cooling phenomena of continuous casting(STEELMAKING, The 113th ISIJ Meeting) (1987)