Search Results1-15 of  15

  • 長谷川 守弘 ID: 9000008344703

    Articles in CiNii:1

    • SUS430連鋳スラブの内部割れについて (1979)
  • 長谷川 守弘 ID: 9000350616781

    日新製鋼周南製鋼所 (1973 from CiNii)

    Articles in CiNii:1

    • 凝固・造塊 (1973)
  • 長谷川 守弘 ID: 9000350616835

    日新製鋼周南製鋼所 (1973 from CiNii)

    Articles in CiNii:1

    • 凝固・造塊 (1973)
  • 長谷川 守弘 ID: 9000350619836

    日新製鋼周南製鋼所 (1974 from CiNii)

    Articles in CiNii:1

    • 物性・反応速度・脱酸 (1974)
  • 長谷川 守弘 ID: 9000350619867

    日新製鋼周南製鋼所 (1974 from CiNii)

    Articles in CiNii:1

    • 物性・反応速度・脱酸 (1974)
  • 長谷川 守弘 ID: 9000410279386

    Articles in CiNii:1

    • Studies of Application of Antimicrobial Stainless Steels for Architecture : Principle of the Antimicrobial Function and Basic Properties of Antimicrobial Stainless Steels I (1997)
  • HASEGAWA Morihiro ID: 9000350604203

    Articles in CiNii:1

    • Synthetic Slag Refining of 18Cr Steel in VOD (1977)
  • HASEGAWA Morihiro ID: 9000350629917

    Articles in CiNii:1

    • Determination of Ultra-low Content of Carbon in Steel by Infrared Absorptiometry after Combustion in Electro Resistance Furnace (1992)
  • HASEGAWA Morihiro ID: 9000350630175

    Articles in CiNii:1

    • Main Factors Affecting Static Holdup of Molten Slag in Coke-packed Bed (1992)
  • HASEGAWA Morihiro ID: 9000350635408

    Articles in CiNii:1

    • Refining of the Solidification Structure of Continuously Cast 18%Cr Stainless Steel by Electromagnetic Stirring (1981)
  • HASEGAWA Morihiro ID: 9000350638321

    Articles in CiNii:1

    • Mechanism of Formation of Surface Defects in Continuously Cast Stainless Steel Slabs Containing Titanium (1987)
  • HASEGAWA Morihiro ID: 9000350649207

    Articles in CiNii:1

    • Tundish Nozzle Constriction in Continuous Casting of Titanium Bearing Stainless Steel Slabs (1984)
  • HASEGAWA Morihiro ID: 9000350650672

    Articles in CiNii:1

    • Kinetics of Nitrogen Desorption from Iron-Chromium Melt under Reduced Pressures (1990)
  • HASEGAWA Morihiro ID: 9000350654432

    Articles in CiNii:1

    • Dephosphorization of Molten Chromium-containing Pig Iron by CaO-CaF<SUB>2</SUB>-FeO Flux with Addition of Li<SUB>2</SUB>CO<SUB>3</SUB> (1983)
  • Hasegawa Morihiro ID: 9000002983476

    Steel & Technology Development Labs., Nisshin Steel Co., Ltd. (1999 from CiNii)

    Articles in CiNii:37

    • Microstructure and Mechanical Properties of Cu Contained Ferritic Stainless Steels (1999)
    • Antimicrobial Activity of Cu Contained Austenitic Stainless Steels (1999)
    • Microstructure and Antimicrobial Activity of Cu Contained Ferritic Stainless Steels (1998)
Page Top