… At current densities lower than 20 A·m<sup>−2</sup>, the content of Fe was approximately 90 mass%, that is, the Zn–Fe alloy exhibited normal co-deposition, whereby the electrochemically more noble Fe deposited preferentially. … At current densities higher than 100 A·m<sup>−2</sup>, however, anomalous co-deposition was observed, whereby the less noble Zn deposited preferentially. …