球状黒鉛鋳鉄における673K脆性の破壊機構と脆化抑制方法 Fracture Mechanism and Suppression Method of 673K Embrittlement in Spheroidal Graphite Cast Irons

この論文にアクセスする

この論文をさがす

著者

抄録

  The effects of chemical composition, microstructure and testing conditions on the so-called 673K embrittlement in spheroidal graphite cast irons were examined in detail. The observation of fracture process shows that the embrittlement is not due to dynamic strain aging (blue embrittlement) but intergranular fracture. It is found that the embrittlement can be suppressed by reducing the Mg/P ratio to less than 1.5.

収録刊行物

  • 鋳造工学 = Journal of Japan Foundry Engineering Society

    鋳造工学 = Journal of Japan Foundry Engineering Society 69(1), 41-48, 1997-01

    公益社団法人 日本鋳造工学会

参考文献:  14件中 1-14件 を表示

  • <no title>

    鋳鉄の高温特性 64,78, 1980

    被引用文献1件

  • <no title>

    Iron Casting Handbook 425, 1981

    被引用文献1件

  • <no title>

    柳沢平

    鋳物 56, 98, 1984

    被引用文献3件

  • <no title>

    呂傳盛

    鋳物講演概要集 113, 20, 1988

    被引用文献1件

  • <no title>

    和泉修

    日本金属学会会報 18, 15, 1979

    被引用文献3件

  • <no title>

    大塚正久

    日本金属学会誌 48, 688, 1984

    被引用文献15件

  • <no title>

    尾中晋

    日本金属学会誌 50, 141, 1986

    被引用文献3件

  • <no title>

    福原吉和

    公開特許公報(昭61-73859)

    被引用文献1件

  • <no title>

    岩渕義孝

    鋳造工学 68, 209, 1996

    被引用文献4件

  • <no title>

    小林良紀

    第90回DCI研究発表会資料, 1994

    被引用文献1件

  • <no title>

    柳沢平

    機械の研究 38, 915, 1986

    被引用文献4件

  • <no title>

    WRIGHT R. N.

    AFS Trans 137, 853, 1985

    被引用文献4件

  • <no title>

    福原吉和

    鋳物講演概要集 109, 9, 1986

    被引用文献5件

  • <no title>

    小林良紀

    鋳物講演概要集 123, 67, 1993

    被引用文献3件

各種コード

  • NII論文ID(NAID)
    10003799814
  • NII書誌ID(NCID)
    AN10514770
  • 本文言語コード
    JPN
  • 資料種別
    ART
  • ISSN
    13420429
  • NDL 記事登録ID
    4118739
  • NDL 雑誌分類
    ZP41(科学技術--金属工学・鉱山工学)
  • NDL 請求記号
    Z17-277
  • データ提供元
    CJP書誌  NDL  J-STAGE 
ページトップへ