抄録

A method to prepare the multi-component oxide glass with graded structure was proposed. This method is based on the facts that colloid particles can sediment during a sol-gel transition process under comparatively low gravity field, and the resultant gel can be converted into glass at lower temperature treatment than a conventional method. The graded structure was formed by centrifuging (10, 000g level) the Si and Ti mixed colloids, and immobilized by removal of solvent at 90°C. This graded precursor gel was heated to 900°C to convert into a glass state. The proper condition to prepare the graded glass was examined especially focusing on the growth time of colloids before the centrifugation. A transparent SiO2-TiO2 glass with molecular-scale graded structure was obtained in many trials.

収録刊行物

被引用文献 (1)*注記

もっと見る

参考文献 (5)*注記

もっと見る

詳細情報 詳細情報について

問題の指摘

ページトップへ