超臨界水環境下における構造用セラミック材料の腐食挙動 [in Japanese] Corrosion Behavior of Structural Ceramics in Supercritical Water [in Japanese]
-
- 長江 正寛 NAGAE Masahiro
- 岡山大学 環境理工学部 Department of Environmental Chemistry and Materials, Faculty of Environmental Science and Technology, Okayama University
-
- 桑江 真一 KUWAE Shinichi
- 岡山大学 環境理工学部 Department of Environmental Chemistry and Materials, Faculty of Environmental Science and Technology, Okayama University
-
- 吉尾 哲夫 [他] YOSHIO Tetsuo
- 岡山大学 環境理工学部 Department of Environmental Chemistry and Materials, Faculty of Environmental Science and Technology, Okayama University
-
- 小田 耕平 ODA Kohei
- 米子工業高等専門学校 物質工学科 Department of Materials Science, Yonago National College of Technology
Search this Article
Author(s)
-
- 長江 正寛 NAGAE Masahiro
- 岡山大学 環境理工学部 Department of Environmental Chemistry and Materials, Faculty of Environmental Science and Technology, Okayama University
-
- 桑江 真一 KUWAE Shinichi
- 岡山大学 環境理工学部 Department of Environmental Chemistry and Materials, Faculty of Environmental Science and Technology, Okayama University
-
- 吉尾 哲夫 [他] YOSHIO Tetsuo
- 岡山大学 環境理工学部 Department of Environmental Chemistry and Materials, Faculty of Environmental Science and Technology, Okayama University
-
- 小田 耕平 ODA Kohei
- 米子工業高等専門学校 物質工学科 Department of Materials Science, Yonago National College of Technology
Journal
-
- Zairyo-to-kankyo
-
Zairyo-to-kankyo 53(11), 526-530, 2004-11-15
腐食防食協会
References: 16
-
1
- <no title>
-
SAKO T.
J. Jpn. Soc. Mech. Eng. 100(946), 24, 1997
Cited by (1)
-
2
- <no title>
-
ARAI K.
Chorinkairyutai-no-Kankyoriyogijutsu, 1999
Cited by (1)
-
3
- <no title>
-
MITTON D. B.
Zairyo-to-Kankyo 49, 130, 2000
Cited by (1)
-
4
- <no title>
-
SAKO T.
Materia jpn. 39(4), 314, 2000
Cited by (1)
-
5
- <no title>
-
KAWASAKI S.
Fundamentals and Applications of Supercritical Fuluids, 2002
Cited by (1)
-
6
- <no title>
-
NAGASE Y.
Fundamentals and Applications of Supercritical Fuluids, 2002
Cited by (1)
-
7
- <no title>
-
KURATA Y.
Materia jpn. 39(4), 320, 2000
Cited by (1)
-
8
- <no title>
-
BOUKIS N.
J.Eur.Ceram.Soc. 17, 71, 1997
Cited by (2)
-
9
- <no title>
-
TANAKA S.
Proceedings of JSCE Materials and Environments 1999, 1999
Cited by (1)
-
10
- <no title>
-
YOSHIO T.
J. Ceram. Soc. Jpn. 96(2), 159, 1988
Cited by (1)
-
11
- <no title>
-
YOSHIO T.
J. Ceram. Soc. Jpn 100(5), 668, 1992
Cited by (1)
-
12
- <no title>
-
YOSHIMURA M.
Met. Technol. 92(2), 52, 1992
Cited by (1)
-
13
- <no title>
-
PROVERBIO E.
J. Eur. Ceram. Soc. 16, 1121, 1996
Cited by (2)
-
14
- <no title>
-
ODA K.
J. Am. Ceram. Soc. 80, 3233-3236, 1997
Cited by (3)
-
15
- <no title>
-
POWELL-DOGAN C. A.
J. Am. Ceram. Soc. 73, 3670-3676, 1990
Cited by (2)
-
16
- Effect of Grain Morphology in Pressureless-Sintered Si<sub>3</sub>N<sub>4</sub>-Y<sub>2</sub>O<sub>3</sub>/Al<sub>2</sub>O<sub>3</sub> on Leaching Behavior under Hydrothermal Conditions [in Japanese]
-
YOSHIO Tetsuo , ODA Kohei , ODA Kiichi
Journal of the Ceramic Association, Japan 95(1100), 435-441, 1987
J-STAGE Cited by (2)