Creation of Fibrous Nanotubes of Green Fluorescent Protein by Conjugation with pH-Responsive Polymer, Poly(2-vinylpyridine), and Use of Microfluidic Synthesis
-
- Naoya Okiyama
- Graduate School of Engineering, Nagoya Institute of Technology
-
- Eriko Ota
- Graduate School of Engineering, Nagoya Institute of Technology
-
- Ayumi Sumino
- Graduate School of Engineering, Nagoya Institute of Technology
-
- Tomoyasu Noji
- Graduate School of Engineering, Nagoya Institute of Technology
-
- Katsuhiro Yamamoto
- Graduate School of Engineering, Nagoya Institute of Technology
-
- Jun-ichi Oku
- Graduate School of Engineering, Nagoya Institute of Technology
-
- Takehisa Dewa
- Graduate School of Engineering, Nagoya Institute of Technology
-
- Toshiki Tanaka
- Graduate School of Engineering, Nagoya Institute of Technology
-
- Toshihisa Mizuno
- Graduate School of Engineering, Nagoya Institute of Technology
この論文をさがす
抄録
<jats:title>Abstract</jats:title> <jats:p>We succeeded in preparing a fibrous nanotube of green fluorescent protein by conjugation with poly(2-vinylpyridine) and use of a microfluidic synthesis technique. By inducing a sudden pH change in the acidic solution (pH 4.5) by injection into a neutral buffer using a microsyringe, the fibrous nanotube could be selectively formed. Its diameter and length were about 200 nm and 1–10 µm, respectively.</jats:p>
収録刊行物
-
- Chemistry Letters
-
Chemistry Letters 42 (5), 495-497, 2013-04-24
Oxford University Press (OUP)
- Tweet
キーワード
詳細情報 詳細情報について
-
- CRID
- 1360283694082072064
-
- NII論文ID
- 10031167802
-
- NII書誌ID
- AA00603318
-
- ISSN
- 13480715
- 03667022
-
- データソース種別
-
- Crossref
- CiNii Articles