書誌事項
- タイトル別名
-
- Influence of Kiln Atmosphere on Color and Sintering Properties of Red Clay Containing Iron
- テツ オ フクム アカツチ ネンド ノ イロ ト ショウケツ トクセイ ニ ロ
この論文をさがす
抄録
Phase transformations of clay containing iron oxide, by firing under various atmospheric conditions up to 1250°C, were studied by X-ray diffraction and ESR. Under reducing conditions and at low temperature (1100°C), hercynite was formed but dissociated at high temperature. Iron oxide was reduced to metallic iron under strongly reducing conditions. The stable phase of hematite appeared when fired in oxidizing atmospheres at 1250°C. Three types of color were observed in the fired products, such as, red in oxidative firing, black in neutral or strongly reductive firing, and yellowish brown in mild reductive firing. Mechanical property was found to be weakest when fired at air ratio of 0.9, that was, under mild reducing condition. This paper describes the effect of atmospheric conditions on firing properties of Japanese clay containing iron oxide for industrial applications.
収録刊行物
-
- 窯業協會誌
-
窯業協會誌 93 (1079), 349-356, 1985
公益社団法人 日本セラミックス協会
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1390001205249754496
-
- NII論文ID
- 110002313404
-
- NII書誌ID
- AN00245650
-
- ISSN
- 18842127
- 00090255
-
- NDL書誌ID
- 3044765
-
- 本文言語コード
- ja
-
- データソース種別
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可