抄録

The relief wear of a noncoated hob grows in the direction of hob rotation. With the increasing of a side relief angle, the width of relief wear geometrically calculated becomes less. In case of a TiN-coated hob, however, a TiN-coating layer restrains the wear from growing in the direction of rotation, and the angle contained by the relief surface and wear surface is large, so a TiN-coated hob is expected to be insensitive to the measuring of a relief angle. As a result of the experiments, (1) a TiN-coated hob is found to be insensitive in measuring the relief angle at a low cutting speed : (2) at a high cutting speed, the smaller relief angle is effective for lengthening the hob life : and therefore, (3) in high-speed and feed hobbing of automobile gears, the relief angle of TiN-coated hob must be as small and as possible.