Electrodeposition of Molybdenum in KF–Na<SUB>2</SUB>B<SUB>4</SUB>O<SUB>7</SUB>–K<SUB>2</SUB>MoO<SUB>4</SUB> Fused Salts
-
- Koyama Koichiro
- Department of Materials Science and Engineering, Himeji Institute of Technology
-
- Hashimoto Yasuhiko
- Department of Materials Science and Engineering, Himeji Institute of Technology
-
- Omori Shinichiro
- Department of Materials Science and Engineering, Himeji Institute of Technology
-
- Terawaki Kazuo
- Graduate Student, Himeji Institute of Technology
書誌事項
- タイトル別名
-
- Electrodeposition of Molybdenum in KF–Na<SUB>2</SUB>B<SUB>4</SUB>O<SUB>7</SUB>–K<SUB>2</SUB>MoO<SUB>4</SUB> Fused Salts
抄録
Smooth, adherent coatings of molybdenum can be obtained electrolytically on nickel and copper substrates in KF–Na2B4O7–K2MoO4 fused salts at temperatures 998–1173 K and current densities 110–550 A/m2 with a molybdenum anode and a graphite anode. The KF–K2MoO4 and Na2B4O7–K2MoO4 fused salts do not give any deposits of metallic molybdenum.
収録刊行物
-
- Transactions of the Japan Institute of Metals
-
Transactions of the Japan Institute of Metals 25 (4), 265-275, 1984
社団法人 日本金属学会
- Tweet
詳細情報 詳細情報について
-
- CRID
- 1390001205118784768
-
- NII論文ID
- 130003486141
-
- COI
- 1:CAS:528:DyaL2cXktFCjsLg%3D
-
- ISSN
- 24324701
- 00214434
-
- 本文言語コード
- en
-
- データソース種別
-
- JaLC
- Crossref
- CiNii Articles
-
- 抄録ライセンスフラグ
- 使用不可