Ironing formability of hard aluminum sheets
-
- USUI Eiki
- Kobe Steel, Co. Ltd., Reserch Department Mooka
-
- INABA Takashi
- Kobe Steel, Co. Ltd., Reserch Department Mooka
Bibliographic Information
- Other Title
-
- アルミニウム硬質材のしごき加工性
- アルミニウム コウシツザイ ノ シゴキ カコウセイ
Search this article
Abstract
Ironing formability of hard aluminum, 1100, 3004 and 5052 sheets was studied. O-temper is prefered to hard temper to ensure a large ironing ratio in single stage ironing. While, hard temper such as H18 is prefered to H2-temper or O-temper, in the tandem stage ironing. These facts are related to the quantity of work hardening before ironing and to the strain hardening coefficient n-vaiue. Intermetailic compounds reduce built-up on a die and reduce friction stress. 3004 alloy is preferable to 1100 or 5052 for ironing. Ironing stress has a minimum value to a half die angle. The lublicating condition has influence to the minimum point. The optimum half die angle for 3004-H18 is about 10°.
Journal
-
- Journal of Japan Institute of Light Metals
-
Journal of Japan Institute of Light Metals 34 (6), 317-324, 1984
The Japan Institute of Light Metals
- Tweet
Details 詳細情報について
-
- CRID
- 1390001206340453376
-
- NII Article ID
- 130004075664
-
- NII Book ID
- AN00069773
-
- ISSN
- 18808018
- 04515994
-
- NDL BIB ID
- 3021590
-
- Text Lang
- ja
-
- Data Source
-
- JaLC
- NDL
- Crossref
- CiNii Articles
-
- Abstract License Flag
- Disallowed