抄録

The microstructure of the aluminum borate whisker reinforced AC8A matrix composite fabricated by squeeze casting was examined with high resolution electron microscopy. Fine reaction products were observed on the whisker surface, which were identified to be MgAl2O4 (partly γ-Al2O3). Those reaction products introduced large strain inside to accomodate the lattice mismatch with a whisker and showed the crystallographic orientation relationship as follows:<br>{010} Al18B4O33//{111} MgAl2O4<br>[001] Al18B4O33//[110] MgAl2O4<br>No further reaction took place at the area covered with the reaction products. Steps were formed on the whisker with the reaction products on them. A thin amorphous-like layer was observed on the interface between the whisker and the matrix.

収録刊行物

  • 軽金属

    軽金属 41 (5), 297-303, 1991

    一般社団法人 軽金属学会

被引用文献 (18)*注記

もっと見る

詳細情報 詳細情報について

問題の指摘

ページトップへ