Effect of a temporary sealing material on the bond strength of CAD/CAM inlay restorations with resin-coating technique

  • UCHIYAMA Saki
    Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University (TMDU)
  • TAKAHASHI Rena
    Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University (TMDU)
  • SATO Takaaki
    Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University (TMDU)
  • ROZAN Shin
    Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University (TMDU)
  • IKEDA Masaomi
    Oral Prosthetic Engineering, Graduate School, Faculty of Dentistry, Tokyo Medical and Dental University (TMDU)
  • INOKOSHI Masanao
    Department of Gerodontology and Oral Rehabilitation, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University (TMDU)
  • NIKAIDO Toru
    Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University (TMDU) Department of Operative Dentistry, Division of Oral Functional Science and Rehabilitation, School of Dentistry, Asahi University
  • TAGAMI Junji
    Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University (TMDU)

この論文をさがす

抄録

<p>This study aimed to assess the effects of a temporary sealing material and cleaning method of resin-coated dentin on the bond strength of computer-aided design/computer-aided manufacturing (CAD/CAM) inlay restorations. Resin-coated dentin surfaces were unsealed or temporarily sealed for 1 h or 1 week. For the temporarily sealed group, a hydraulic temporary sealing material was removed and further divided into four groups: without cleaning, cleaned with a rotational brush, a universal cleaner or an air-polishing device. Some specimens were investigated with energy dispersive X-ray spectroscopy and the others were used for microtensile bond strength (MTBS) test. A sealing material could not be removed with a rotational brush, which resulted in pretest failures in all specimens after 1 h and which resulted in low MTBS after 1 week. An air-polishing device can clean resin-coated dentin temporarily sealed with a hydraulic temporary sealing material and resulted in the similar MTBS as in the unsealed group.</p>

収録刊行物

  • Dental Materials Journal

    Dental Materials Journal 40 (5), 1122-1128, 2021-09-25